Cold Weldable
Max Temp: 600°C
Material: Al (99.5)
Volume: 85 μl
Diameter: ø 6.7 mm
| Part Number | Description | Type | Diameter | Details |
| DSC21400A66.050-00 | 30/40 μl, 100 pcs | Concavus | ø 5 mm | |
| 6.239.2-64.8.00 | 40 μl, 100 pcs | ø 6 mm | Set of 100 pcs., cold weldable** | |
| 6.239.2-64.81.00 | 40 μl. 500 pcs | ø 6 mm | Set of 500 pcs., cold weldable** |