| Part Number | Description | Material | Max Temp | Additional Details | Additional Accessories | Link |
| 6.214.5-91.6.00 | n/a | Glassy Carbon | 2000°C | Set of O-rings included. Inert atmosphere | ||
| 6.214.5-90.1.00 | Normal Atmosphere Supplement | Al2O3 | 1680°C | Set of seals, insulating parts and gas plug connections included. Inert, oxidizing atmosphere. | ||
| 6.214.5-91.1.00 | O-rings and Protective Tube Only | Al2O3 | 1680°C | Set of O-rings included, spare part for 6.214.5-90.1.00. Inert, oxidizing atmosphere. | 6.214.5-90.1.00 |