Diameter (mm): 14
| Part Number | Description | Product Details | Additional Accessories | Link |
| KNX0027-SB | Surface Finish: Roughened (Sandblasted) Material: Stainless Steel | Closed base design. | Bob upper geometry of same or smaller diameter | |
| KNX2040 | Surface Finish: Smooth Material: Anodized Aluminum | DIN Standard. Removable Push-ft Base | ||
| KNX2512 | Surface Finish: Smooth Material: Stainless Steel | Removable Screw Base | ||
| KNX2084 | Surface Finish: Splined Material: Aluminum | Hard anodized aluminium cup insert. Removable Push-Fit Base | Bob upper geometry of same or smaller diameter |