Furnace temps:
400C, 1300C, 1575C, 2000C
Sample holder set, pressure-calibrated sample holder; pressure up to 5 MPa; 3-layer analysis; including torque wrench for 60 ...260 Ncm; maximum working temperature of 300°C
Log in with approved account
Furnace temps:
400C, 1300C, 1575C, 2000C
Sample holder set, pressure-calibrated sample holder; pressure up to 5 MPa; 3-layer analysis; including torque wrench for 60 ...260 Ncm; maximum working temperature of 300°C

Our Thermal Analysis Applications Laboratories are a experienced partner for thermal analysis issues. Our involvement in your projects begins with precise and careful sample preparation and continues through profound examination and interpretation of the measurement results.