Not ASC Compatible
| Part Number | Description | Product Details | Additional Accessories | Link |
| HTP40000A64.010-00 | Temp Range (℃): 25 to 1100 (Type S - Fused Silica), Not ASC Compatible | Made of fused silica, type S. Crucible required: Fused silica, 3.4 ml, NGB811507 | NGB811507 | |
| HTP40000A64.000-00 | Temp Range (℃): 25 to 1100 (Type S - Fused Silica), Not ASC Compatible | Made of fused silica, type S. Crucible required: Fused silica, 3.4 ml, NGB811507 | NGB811507 | |
| HTP40000A58.010-00 | Temp Range (℃): 25 to 1650 (Type S), Not ASC Compatible | |||
| HTP40000A58.000-00 | Temp Range (℃): 25 to 1650 (Type S), Not ASC Compatible | Includes Al2O3, 3.4 ml, GB445213 | GB445213 | |
| HTP40000A62.010-00 | Temp Range (℃): 25 to 1650 (Type W - Al2O3), Not ASC Compatible | Made of Al2O3, W3%Re/W25%Re | ||
| HTP40000A62.000-00 | Temp Range (℃): 25 to 1650 (Type W - Al2O3), Not ASC Compatible | Made of Al2O3, W3%Re/W25%Re. Includes Al2O3, 3.4 ml, GB445213 | GB445213 |