| Part Number | Description | Max Temp | Volume | Quantity | Diameter | Details | Additional Accessories | Link |
| NGB812639 | MgO | 1500℃ | 85 μl | Min 10 pcs | ø 6.7 mm | NGB812637 | ||
| NGB808836 | BN | 1600℃ | 85 μl | ø 6.7 mm | Inert gas required | NGB808835 | ||
| NGB812636 | Y2O3 | 1700℃ | 85 μl | ø 6.7 mm | NGB812635 | |||
| NGB808165 | Mo | 2000℃ | 85 μl | ø 6.4 mm | NGB820241 | |||
| GB397053 | ZrO2 | 2000℃ | 85 μl | CaO Stabilized | GB397052 | |||
| NGB811386 | Glassy Carbon | 2400℃ | 85 μl | ø 6 mm | NGB812613 | |||
| GB399956 | Graphite | 2400℃ | 85 μl | T > 2200 C evaporation may occur | GB399957 | |||
| 6.239.2-64.5.01 | Al (99.5) | 600°C | 25/40 μl | 100 pcs. | ø 6 mm | 100 pieces | 6.239.2-64.5.02 |