| Part Number | Description | Max Temp | Diameter | Details | Additional Accessories | Link |
| GB280062 | Material : Pt/Ir, Volume: 0.3 ml, | 1600℃ | GB280066 | |||
| GB399147 | Material : Al2O3, Volume: 0.15 ml, | 1700℃ | TGA-DTA Sample Carrier A53 | GB399973 | ||
| GB445172 | Material : Al2O3, Volume: 0.2 ml, | 1700℃ | GB445175 | |||
| NGB810411 | Material : Al2O3, Volume: 0.3 ml, Quantity: 100 pcs, | 1700℃ | GB445175 | |||
| NGB813974 | Material : Al2O3, Volume: 0.3 ml | 1700℃ | ø 6 mm | Sixfold pierced | ||
| NGB815846 | Material : Y2O3, Volume: 0.15 ml, | 1700℃ | Not useable in contact with Al2O3; TGA-DTA Sample Carrier A53 | |||
| NGB820035 | Material : Al2O3 (Highly Sintered), Volume: 0.3 ml, Quantity: 100 pcs, | 1750℃ | Highly sintered | NGB820036 | ||
| GB395116 | Material : Glassy Carbon, Volume: 60 µl, | 2000℃ | Up to 500°C stable in oxidizing atmosphere; TGA-DTA Sample Carrier A53 | |||
| GB399148 | Material : ZrO2, Volume: 0.15 ml, | 2000℃ | TGA-DTA Sample Carrier A53 | |||
| GB427607 | Material : Graphite, Volume: 0.15 ml, | 2400℃ | TGA-DTA Sample Carrier A53 | NGB814940 | ||
| GB399222 | Material : Graphite, Volume: 0.3 ml, | 2400℃ | T > 2200°C evaporation may occur | |||
| GB453520 | Material : Tungsten, Volume: 80 µl, | 2400℃ | Wall thickness 0.3 mm, only for STA 449 F3 Jupiter®; TGA-DTA Sample Carrier A53 | |||
| NGB808999 | Material : Tungsten, Volume: 80 µl, | 2400℃ | Wall thickness 0.2 mm, BN liner available; TGA-DTA Sample Carrier A53 | NGB809406 | ||
| GB440112 | Material : Fine Steel, Volume: 0.3 ml, | 600℃ | Only in inert atmosphere | GB440113 |
Crucible - DTA, STA
Log in with approved account

Contract Testing
Our Thermal Analysis Applications Laboratories are a experienced partner for thermal analysis issues. Our involvement in your projects begins with precise and careful sample preparation and continues through profound examination and interpretation of the measurement results.