Max Length: 52 mm
Tube ø: 12 mm
Set of Sample Supports Included: 4, 6, 8 mm
| Part Number | Max Temperature (℃) | Thermocouple Type | Description |
| DIL40200A62.000-00 | 1680°C | Type B | Highly sintered Al2O3. Includes holding tube with metal bush, slide, pushrod, thermocouple holding segment, thermocouple and a set of sample supports. |
| DIL40200A66.000-00 | 1000°C | Type K | Includes holding tube with metal bush, slide, pushrod, thermocouple holding segment, thermocouple and a set of sample supports. |

