| Part Number | Description | Diameter | Thickness | Melting Temp | Short Description |
| 6.219.1-92.5.00 | Al2O3 50mm length | 6 mm | 4 mm | 1680°C | High-purity, polycrystalline, manufacturer´s certificate included. Reaction may occur between Al2O3/sapphire and graphite at temperatures above 1400°C. |
| 6.219.1-92.2.00 | Al2O3 25mm length | 6 mm | 1680°C | High-purity, polycrystalline, manufacturer´s certificate included. Reaction may occur between Al2O3/sapphire and graphite at temperatures above 1400°C. | |
| 6.217.1-91.2.00 | Al2O3 20mm length | 6 mm | 1680°C | High-purity, polycrystalline, manufacturer´s certificate included. Reaction may occur between Al2O3/sapphire and graphite at temperatures above 1400°C. | |
| 6.219.1-92.11.00 | Al2O3 15mm length | 1680°C | High-purity, polycrystalline, manufacturer´s certificate included. Reaction may occur between Al2O3/sapphire and graphite at temperatures above 1400°C. | ||
| 6.219.1-92.7.00 | Al2O3 12mm length | 6 mm | 1680°C | High-purity, polycrystalline, manufacturer´s certificate included. Reaction may occur between Al2O3/sapphire and graphite at temperatures above 1400°C. | |
| 6.219.1-92.10.00 | Al2O3 10mm length | 6 mm | 1680°C | High-purity, polycrystalline, manufacturer´s certificate included. Reaction may occur between Al2O3/sapphire and graphite at temperatures above 1400°C. | |
| 6.219.1-92.14.00 | Al2O3 5mm length | 6 mm | 1680°C | High-purity, polycrystalline, manufacturer´s certificate included. Reaction may occur between Al2O3/sapphire and graphite at temperatures above 1400°C. | |
| 6.214.1-91.1.00 | Fused Silica 50mm length | 6 mm | 1100°C | Expansion table and purity certificate included | |
| 6.216.0-91.1.00 | Fused Silica 25mm length | 6 mm | 1100°C | Expansion table and purity certificate included | |
| 6.219.1-92.8.00 | Fused Silica 12mm length | 6 mm | 1100°C | Expansion table and purity certificate included | |
| 6.219.1-92.16.00 | Fused Silica 10mm length | 6 mm | 1100°C | Expansion table and purity certificate included | |
| 6.216.0-91.8.00 | Platinum 25mm length | 4 mm | 1000°C | Expansion table included | |
| 6.216.0-91.7.00 | Poco Graphite 25mm length | 6 mm | 2800°C | Expansion table included | |
| 6.219.1-92.6.00 | Sapphire 50mm length | 6 mm | 1680°C | Manufacturer´s certificate included. Reaction may occur between Al2O3/sapphire and graphite at temperatures above 1400°C. | |
| 6.219.1-92.3.00 | Sapphire 25mm length | 6 mm | 1680°C | Manufacturer´s certificate included. Reaction may occur between Al2O3/sapphire and graphite at temperatures above 1400°C. | |
| 6.219.1-92.9.00 | Sapphire 12mm length | 6 mm | 1680°C | Manufacturer´s certificate included. Reaction may occur between Al2O3/sapphire and graphite at temperatures above 1400°C. | |
| 6.216.0-91.6 | Tungsten 25mm length | 6 mm | 2400°C | Expansion table included |
DIL, TMA - Reference Material - Expansion