| Part Number | Description | Melting Temp | Details |
| 6.223.5-91.3.05 | Aluminum wire | 660.3 ℃ | Calibration standard in Glass Vials; 400 mg; D = 1 mm |
| 6.223.5-91.3.04 | Bismuth | 271.4 ℃ | Calibration standard in Glass Vials; 400 mg |
| 6.223.5-91.3.07 | Gold wire | 1064.2 ℃ | Calibration standard in Glass Vials; 400 mg; D = 1.0 mm |
| 6.223.5-91.3.01 | Indium | 156.6 ℃ | Calibration standard in Glass Vials; 400 mg |
| 6.223.5-91.3.06 | Silver wire | 961.8 ℃ | Calibration standard in Glass Vials; 400 mg; D = 0.5 mm |
| 6.223.5-91.3.02 | Tin | 231.9 ℃ | Calibration standard in Glass Vials; 400 mg |