6.223.5-91.3.05 Aluminum wire 660.3 ℃ Calibration standard in Glass Vials; 400 mg; D = 1 mm
6.223.5-91.3.04 Bismuth 271.4 ℃ Calibration standard in Glass Vials; 400 mg
6.223.5-91.3.07 Gold wire 1064.2 ℃ Calibration standard in Glass Vials; 400 mg; D = 1.0 mm
6.223.5-91.3.01 Indium 156.6 ℃ Calibration standard in Glass Vials; 400 mg
6.223.5-91.3.06 Silver wire 961.8 ℃ Calibration standard in Glass Vials; 400 mg; D = 0.5 mm
6.223.5-91.3.02 Tin 231.9 ℃ Calibration standard in Glass Vials; 400 mg
6.223.5-91.3.03 Zinc 419.5 ℃ Calibration standard in Glass Vials; 400 mg
Contract Testing

Contract Testing

Our Thermal Analysis Applications Laboratories are a experienced partner for thermal analysis issues. Our involvement in your projects begins with precise and careful sample preparation and continues through profound examination and interpretation of the measurement results.

Learn More
Have Questions?

Have Questions?

Our experts are happy to help you.

Contact Us