Image coming soon

LFA Reference Materials - Thermal Diffusivity & Specific Heat (Cp) - Inconel 600

Write a Review
Part Number Shape Diameter / Width (mm) Thickness (mm) Short Description
6.256.4-93.1.04 Round 25.4 2.5 a @ RT = 3.458 mm2/s
6.256.4-93.9.04 Round 20.0 2.5 a @ RT = 3.458 mm2/s
6.256.4-93.2.04 Round 12.7 2.5 a @ RT = 3.458 mm2/s
6.256.4-93.10.04 Square 12.7 x 12.7 2.5 a @ RT = 3.458 mm2/s
6.256.4-93.3.04 Round 10.0 2.0 a @ RT = 3.458 mm2/s
6.256.4-93.6.04 Square 10.0 x 10.0 2.0 a @ RT = 3.458 mm2/s
6.256.4-93.7.02 Square 8.0 x 8.0 2.0  
6.256.4-93.1.01 Round 25.4 1.0  
6.256.4-93.2.01 Round 12.7 1.0  
6.256.4-93.3.01 Round 10.0 1.0  
6.256.4-93.6.01 Square 10.0 x 10.0 1.0  
6.256.4-93.7.01 Square 8.0 x 8.0 1.0  
Contract Testing

Contract Testing

Our Thermal Analysis Applications Laboratories are a experienced partner for thermal analysis issues. Our involvement in your projects begins with precise and careful sample preparation and continues through profound examination and interpretation of the measurement results.

Learn More
Have Questions?

Have Questions?

Our experts are happy to help you.

Contact Us