a @ RT = 54.3 mm2/s
| Part Number | Description | Shape | Thickness | Details |
| 6.256.4-98.2.04 | 12.7mm dia | Round | 2.5mm | a @ RT = 69.3 mm2/s |
| 6.256.4-98.3.02 | 10.0mm dia | Round | 2.0mm | a @ RT = 69.3 mm2/s |
| 6.256.4-98.10.04 | 12.7 x 12.7mm | Square | 2.5mm | a @ RT = 69.3 mm2/s |
| 6.256.4-98.6.02 | 10.0 x 10.0mm | Square | 2.0mm | a @ RT = 69.3 mm2/s |