LFA Reference Materials - Thermal Diffusivity & Specific Heat (Cp) - Tungsten

Write a Review

a @ RT = 54.3 mm2/s

Part Number Description Shape Thickness Details
6.256.4-98.2.04 12.7mm dia Round 2.5mm a @ RT = 69.3 mm2/s
6.256.4-98.3.02 10.0mm dia Round 2.0mm a @ RT = 69.3 mm2/s
6.256.4-98.10.04 12.7 x 12.7mm Square 2.5mm a @ RT = 69.3 mm2/s
6.256.4-98.6.02 10.0 x 10.0mm Square 2.0mm a @ RT = 69.3 mm2/s

 

Contract Testing

Contract Testing

Our Thermal Analysis Applications Laboratories are a experienced partner for thermal analysis issues. Our involvement in your projects begins with precise and careful sample preparation and continues through profound examination and interpretation of the measurement results.

Learn More
Have Questions?

Have Questions?

Our experts are happy to help you.

Contact Us