| Part Number | Description | Product Details |
| HTP40000A59.010-00 | Temp Range (℃): -150 to 1000 (Type P), Not ASC Compatible, No Radiation shield included, Shape: n/a | |
| HTP40000A59.000-00 | Temp Range (℃): -150 to 1000 (Type P), Not ASC Compatible, Radiation shield included, Shape: n/a | |
| HTP40000A70.010-00 | Temp Range (℃): -150 to 700 (Type E), Not ASC Compatible, No Radiation shield included, Shape: Standard | Inert: -150 to 700; Oxidizing: -150 to 500 |
| HTP40000A79.010-00 | Temp Range (℃): -150 to 700 (Type E), Not ASC Compatible, No Radiation shield included, Shape: Octagonal | Octagonal; Inert: -150 to 700; Oxidizing: -150 to 500 |
| HTP40000A70.000-00 | Temp Range (℃): -150 to 700 (Type E), Not ASC Compatible, Radiation shield included, Shape: Standard | Inert: -150 to 700; Oxidizing: -150 to 500 |
| HTP40000A79.000-00 | Temp Range (℃): -150 to 700 (Type E), Not ASC Compatible, Radiation shield included, Shape: Octagonal | Octagonal; Inert: -150 to 700; Oxidizing: -150 to 500 |
| HTP40000A71.010-00 | Temp Range (℃): -150 to 800 (Type K), Not ASC Compatible, No Radiation shield included, Shape: Standard | Inert: -150 to 800; Oxidizing: -150 to 500 |
| HTP40000A77.010-00 | Temp Range (℃): -150 to 800 (Type K), Not ASC Compatible, No Radiation shield included, Shape: Octagonal | Octagonal; Inert: -150 to 800; Oxidizing: -150 to 500 |
| HTP40000A71.000-00 | Temp Range (℃): -150 to 800 (Type K), Not ASC Compatible, Radiation shield included, Shape: Standard | Inert: -150 to 800; Oxidizing: -150 to 500 |
| HTP40000A77.000-00 | Temp Range (℃): -150 to 800 (Type K), Not ASC Compatible, Radiation shield included, Shape: Octagonal | Octagonal; Inert: -150 to 800; Oxidizing: -150 to 500 |
| HTP40000A54.010-00 | Temp Range (℃): 25 to 1650 (Type S), Not ASC Compatible, No Radiation shield included, Shape: Round - For Cp | Round Design Cp |
| HTP40000A69.010-00 | Temp Range (℃): 25 to 1650 (Type S), Not ASC Compatible, No Radiation shield included, Shape: Standard | |
| HTP40000A72.010-00 | Temp Range (℃): 25 to 1650 (Type S), Not ASC Compatible, No Radiation shield included, Shape: Standard - For Cp | Cp |
| HTP40000A78.010-00 | Temp Range (℃): 25 to 1650 (Type S), Not ASC Compatible, No Radiation shield included, Shape: Octagonal - For Cp | Octagonal Cp |
| HTP40000A54.000-00 | Temp Range (℃): 25 to 1650 (Type S), Not ASC Compatible, Radiation shield included, Shape: Round - For Cp | Round Design Cp |
| HTP40000A69.000-00 | Temp Range (℃): 25 to 1650 (Type S), Not ASC Compatible, Radiation shield included, Shape: Standard | |
| HTP40000A72.000-00 | Temp Range (℃): 25 to 1650 (Type S), Not ASC Compatible, Radiation shield included, Shape: n/a | Cp |
| HTP40000A78.000-00 | Temp Range (℃): 25 to 1650 (Type S), Not ASC Compatible, Radiation shield included, Shape: n/a | Octagonal Cp |
| HTP40000A76.010-00 | Temp Range (℃): 25 to 1750 (Type B), Not ASC Compatible, No Radiation shield included, Shape: n/a | |
| HTP40000A76.000-00 | Temp Range (℃): 25 to 1750 (Type B), Not ASC Compatible, Radiation shield included, Shape: n/a | |
| HTP40000A63.010-00 | Temp Range (℃): -150 to 1000 (Type P), ASC Compatible, No Radiation shield included, Shape: n/a | For ASC |
| HTP40000A63.000-00 | Temp Range (℃): -150 to 1000 (Type P), ASC Compatible, Radiation shield included, Shape: n/a | For ASC |
| HTP40000A66.010-00 | Temp Range (℃): -150 to 700 (Type E), ASC Compatible, No Radiation shield included, Shape: n/a | Inert: -150 to 700; Oxidizing: -150 to 500 |
| HTP40000A66.000-00 | Temp Range (℃): -150 to 700 (Type E), ASC Compatible, Radiation shield included, Shape: n/a | Inert: -150 to 700; Oxidizing: -150 to 500 |
| HTP40000A74.010-00 | Temp Range (℃): -150 to 700 (Type: K), ASC Compatible, No Radiation shield included, Shape: n/a | Inert: -150 to 800; Oxidizing: -150 to 500 |
| HTP40000A74.000-00 | Temp Range (℃): -150 to 700 (Type: K), ASC Compatible, Radiation shield included, Shape: n/a | Inert: -150 to 800; Oxidizing: -150 to 500 |
| HTP40000A73.010-00 | Temp Range (℃): 25 to 1650 (Type S), ASC Compatible, No Radiation shield included, Shape: For Cp | For ASC |
| HTP40000A75.010-00 | Temp Range (℃): 25 to 1650 (Type S), ASC Compatible, No Radiation shield included, Shape: Not For Cp | |
| HTP40000A73.000-00 | Temp Range (℃): 25 to 1650 (Type S), ASC Compatible, Radiation shield included, Shape: For Cp | For ASC |
| HTP40000A75.000-00 | Temp Range (℃): 25 to 1650 (Type S), ASC Compatible, Radiation shield included, Shape: Not For Cp | |
| HTP40000B73.000-00 | Temp Range (℃): 25 to 1750 (Type B), ASC Compatible, Radiation shield included, Shape: n/a | For ASC |