Max Length: 52 mm
| Part Number | Description | Product Details | Max Temp (℃) |
| DIL40200A50.000-00 | Single Al2O3 12mm Sample ø - 4, 6, 8 mm sample supports included, Type S Thermocouple | Highly sintered Al2O3. Allowing for samples of various diameters to be measured over a wide temperature range. | 1680°C |
| DIL40200A52.000-00 | Single Fused Silica 19 mm Sample ø - 6, 12.7, 15 mm sample supports included, Type K thermocouple | Includes holding tube with metal bush, slide, pushrod, thermocouple holding segment, thermocouple and a set of sample supports. | 1100°C |
| DIL40200A68.000-00 | Single Graphite 6 mm Sample ø - 4, 6, 8 mm sample supports included, Type W Thermocouple | Thermocouple W3%Re-W25%Re. Includes holding tube with metal bush, slide, pushrod, thermocouple holding segment, thermocouple and a set of sample supports. The longitudinal temperature distribution is optimized to the available standard samples of maximum 25 mm. | 2000°C |
| DIL40200A78.000-00 | Single Graphite5 6 mm Sample ø - 4, 6 mm sample supports included, Type W Thermocouple | With sheathed W3%Re-W25%Re thermocouple; sheath made of molybdenum. Includes holding tube with metal bush, slide, pushrod, thermocouple holding segment, thermocouple and a set of sample supports. The longitudinal temperature distribution is optimized to the available standard samples of maximum 25 mm. | 2000°C |
| DIL40200A72.000-00 | Single Graphite 19 mm Sample ø - 6, 12.7, 15 mm sample supports included, Type W Thermocouple | Thermocouple W3%Re-W25%Re. Includes holding tube with metal bush, slide, pushrod, thermocouple holding segment, thermocouple and a set of sample supports. The longitudinal temperature distribution is optimized to the available standard samples of maximum 25 mm. | 2000°C |
| DIL40200A77.000-00 | Single Graphite 8 mm Sample ø - 4, 6, 8 mm sample supports included, Type W thermocouple | Pyrometer, thermocouple W3%Re-W25%Re. Includes holding tube with metal bush, slide, pushrod, thermocouple holding segment, thermocouple and a set of sample supports. The longitudinal temperature distribution is optimized to the available standard samples of maximum 25 mm. | 2800°C |
| DIL40200A55.000-00 | Single Graphite 19 mm Sample ø - 6, 12.7, 15 mm sample supports included, Type W Thermocouple | Pyrometer, thermocouple W3%Re-W25%Re. Includes holding tube with metal bush, slide, pushrod, thermocouple holding segment, thermocouple and a set of sample supports. The longitudinal temperature distribution is optimized to the available standard samples of maximum 25 mm. | 2800°C |